Micatemp Machinable Glass/Mica Ceramic Composite are designed for electro-mechanical and thermo-mechanical applications requiring one or more of the following properties: good machinability, excellent resistance to heat and/or open flame up to 1832ºF (1000ºC), low thermal conductivity, excellent electrical insulation, extremely high resistance to pressure, high resistance to impact (cracking, and chipping), impervious to most chemicals (including oil, grease, and water), asbestos-free, and ecologically safe and non-toxic.

Specifications

FlammabilityDoes not burn
Moisture AbsorptionNil
Hardness - Rockwell H ( H )90
Hardness - Brinell ( H )56
Density ( lb/in³ )0.09
Flexural Strength ( psi )13000
Specific Gravity2.5
Coefficient of Thermal Expansion ( in/in/ºF )5.8 x 10-6
Coefficient of Thermal Expansion ( in/in/ºC )10.5 x 10-6
Tensile Strength ( psi )6000
Compressive Strength ( psi )45000
Arc Resistance ( sec )300
Thermal Conductivity ( BTU-in/hr-ft²-ºF )0.00100
Thermal Conductivity ( cal cm/secell namem² ºF )0.24
Dielectric Constant ( MHz )6.7
Specific Heat ( cal/g/ºC )0.12
IZOD Impact Strength ( ft lb/in )1.8
Maximum Continuous Operating Temperature ( ºC )400
Maximum Continuous Operating Temperature ( ºF )750
Mica FillerNatural
Radiation Resistance (3 x 1010 Rods-Cobalt)Good
Dielectric Strength (1/8" Thick) ( V/mil )400
Permittivity ( MHz )6.7
Dissipation Factor ( MHz )0.0018
Loss Index ( MHz )0.012
Dry Surface Resistivity at (70ºF) ( ohm-cm )1016
Volume Resistivity at 70ºF ( ohm-cm )1012
Wet Surface Resistivity at (70ºF) ( ohm-cm )106
Modulus of Elasticity (in Tension) ( psi )11.0 x 106